2021-10-11 17:04:07
High-speed jet into the crushing chamber, collides with particles, multiple times in the friction of high pressure air, shear pulverization, pulverized materials, and the assembly of rising airflow motion, in the fan Under the action, the powerful centrifugal force of the rotational speed of FL Multiple-stage Classifier IN Series of Psticides, the thickness of the material and the separation of the fine particles enter the cyclone separator and dust removal, the crude particles continue to be pulverized . The classifier produced by AlPa can perform local internal changes depending on the different characteristics of the material, so that it is more suitable for the grading requirements of the material. The grading machine has a greater amount of processing, energy saving, simple operation, and low maintenance costs.
FL Multiple-stage Classifier In Series Of Pesticides Using Materials Under the action of high-speed airflow, the high-speed collision and the severe friction between the high-speed collision and the particles are caused in the pulverization chamber, and the high-speed airflow generates shear. The purpose is to achieve the purpose of pulverization.How to continue FL MultiPle-Stage Classifier In Series Of Pesticides? Here are the following aspects: 1. In the production process, the temperature rise of the bearing must be regularly checked. When the temperature rises to 50 ° C, the inspection should be checked, find a reason, and troubleshoot the fault. 2. When the new machine is running, the transmission belt is easily stretched, and the tightness of the belt should be adjusted to ensure the life of the belt. 3. Regularly check the lifting parts, promptly guarantee the quality of production and production. 4, blade and bushing should always check the wear situation. When wear, the productivity is lowered, and the grain is thick. 5, the host and gradient flow bearing oil grease lubrication, the use of special grease, and the degree of 265-295.6, and the change cycle of the bearing is 2000 hours. The amount of the grease is filled into a 1/2 (upper test) or 3/4 (below the test), so we can't add too much grease. Otherwise, the bearing temperature is too high. 7, the spiral feeder is 4,000 hours, plus ordinary calcium based grease.